云南某有色金属伴生铁尾矿氢基矿相转化工艺研究
黄瑞 , 余裕森 , 李文博 , 唐志东 , 谢恩龙 , 高起方
有色金属(选矿部分) ›› 2026, Vol. 0 ›› Issue (8) : 317 -324.
云南某有色金属伴生铁尾矿氢基矿相转化工艺研究
Research on Hydrogen-Based Mineral Phase Transformation Process for Iron Tailings Associated with Non-ferrous Metals in Yunnan
伴随高品位铁矿资源持续消耗, 低品位、组成复杂且难选铁矿资源的高效利用愈发重要。针对云南某有色金属伴生铁尾矿开展研究, 该尾矿原矿铁品位为14. 13%, 含铁矿物以菱铁矿和褐铁矿为主, 脉石矿物则以石英为主, 采用常规选矿方法难以直接得到合格铁精矿。首先通过强磁选对尾矿进行预富集, 得到铁品位为21. 72% 的预富集产物;在此基础上, 进一步实施氢基矿相转化-磁选试验, 系统考察焙烧温度、焙烧时间、H2 浓度、焙烧后磨矿细度及磁场强度对分选效果的影响。同时结合SEM、XRD 及VSM 等手段, 对样品的微观结构演变、矿物物相转化行为和磁性变化特征等进行分析。结果表明:当给料中-0. 038 mm 粒级含量占50%, 焙烧温度为580 ℃、焙烧时间为30 min、H2 浓度为40%、焙烧产品磨矿细度-0. 038 mm 粒级含量占70%、磁场强度为0. 132 T 时, 所得铁精矿中铁品位和铁回收率分别达到61. 39% 和65. 11%。研究结果可为有色金属伴生难选铁尾矿的资源化利用提供试验依据。
With the continuous consumption of high-grade iron ore resources, the efficient utilization of low-grade, complex, and refractory iron ore resources is becoming increasingly important. A study was conducted on a nonferrous-metal-associated iron tailings from Yunnan. The raw tailings had an iron grade of 14. 13%, with siderite and limonite as the main iron-bearing minerals and quartz as the predominant gangue mineral. It is difficult to directly obtain a qualified iron concentrate using conventional beneficiation methods. First, the tailings were pre-concentrated by high-intensity magnetic separation, yielding a pre-concentrate with an iron grade of 21. 72%. On this basis, hydrogen-based mineral phase transformation-magnetic separation tests were carried out to systematically investigate the effects of roasting temperature, roasting time, H2 concentration, grinding fineness after roasting, and magnetic field intensity on the separation performance. Meanwhile, the microstructural evolution, mineral phase transformation behavior, and magnetic property changes of the samples were analyzed by means of SEM, XRD, and VSM. The results showed that when the feed contained 50% -0. 038 mm material, the roasting temperature was 580 ℃, the roasting time was 30 min, the H2 concentration was 40%, the roasted product was ground to 70% passing 0. 038 mm, and the magnetic field intensity was 0. 132 T, the obtained iron concentrate achieved an iron grade of 61. 39% and an iron recovery of 65. 11%. The findings can provide an experimental basis for the resource utilization of refractory iron tailings associated with nonferrous metals.
| [1] |
韩跃新, 高鹏, 李艳军, |
| [2] |
|
| [3] |
张铃, 路永森, 薛晨, |
| [4] |
|
| [5] |
柳林, 王威, 刘红召, |
| [6] |
|
| [7] |
姜亚雄, 黄丽娟, 黄恩旭, |
| [8] |
|
| [9] |
曾永杰, 刘文丽, 樊庆龙, |
| [10] |
|
| [11] |
张婉悦, 余建文, 韩跃新, |
| [12] |
|
| [13] |
韩跃新, 张小龙, 高鹏, |
| [14] |
|
| [15] |
聂琪, 朱宁, 张汉平, |
| [16] |
|
| [17] |
张宗旺, 李健, 李燕, |
| [18] |
|
| [19] |
罗立群, 乐毅. 难选铁物料磁化焙烧技术的研究与发展[J]. 中国矿业, 2007, 16(3): 55-58. |
| [20] |
|
| [21] |
刘兴华, 罗良飞, 刘卫, |
| [22] |
|
| [23] |
周廷波, 魏晓彤, 孙永升, |
| [24] |
|
| [25] |
姜亚雄, 汪勇, 祁磊, |
| [26] |
|
| [27] |
孔德翠, 刘杰, 张淑敏, |
| [28] |
|
国家自然科学基金区域创新发展联合基金重点项目(U24A2093)
/
| 〈 |
|
〉 |